Polyacrylic elastic injection resin for permanent watertight sealing Sika® Injection-304 is a very low viscous, elastic and very quick-gelling polyacrylic injection resin with a gelling time adjustable within a range. The material reacts to form a waterproof, elastic and solid gel with good adhesion to both dry and wet substrates. - Permanently elastic
- Capable of reversibly absorbing (swelling) and releasing (shrinking) moisture
- Adjustable gelling times at various temperature ranges
- Very low viscosity compared to water
- Once cured the Product is insoluble in water and hydrocarbons and resistant to alkalis
- Resistant to alternating freeze and thaw exposure
- Injected with a two component pump
|
Usage The Product is designed for: - Sealing of all types of leaking building components in damp or water saturated ground
- Curtain injection
- Consolidation of non-cohesive soils with low permeability
Please note: - The Product must only be used in below ground structures
Advantages - Permanently elastic
- Capable of reversibly absorbing (swelling) and releasing (shrinking) moisture
- Adjustable gelling times at various temperature ranges
- Very low viscosity compared to water
- Once cured the Product is insoluble in water and hydrocarbons and resistant to alkalis
- Resistant to alternating freeze and thaw exposure
- Injected with a two component pump
Packaging Part A1 (Resin) | 21.5 kg | Part A2 (Accelerator) | 1.05 kg | Part B ( Hardener) | 1.00 kg |
Refer to the current price list for available packaging variations. Colour Part A1 (Resin) | Amber - liquid | Part A2 (Accelerator) | Colourless - liquid | Part B (Hardener) | White powder | |
Application Information Mixing Ratio A = A1 : A2 | 21.5 : 1.05 parts by weight | B solution = water : B | 20 : 1 parts by weight (Standard mixture) | A : B solution | 1 : 1 parts by volume | Ambient Air Temperature Maximum | +40 °C | Minimum | +5 °C | Substrate Temperature Maximum | +40 °C | Minimum | +5 °C | Reaction time Reference values depend on the concentration of Part B at various application temperatures. B : Water = 0,5 % by weight Material Temperature | Increase in viscosity | Reaction time | +10 °C | ~220 s | ~315 s | +20 °C | ~103 s | ~180 s |
B : Water = 1,0 % by weight Material Temperature | Increase in viscosity | Reaction time | +10 °C | ~150 s | ~225 s | +20 °C | ~72 s | ~150 s |
B : Water = 2,0 % by weight Material Temperature | Increase in viscosity | Reaction time | +10 °C | ~85 s | ~150 s | +20 °C | ~45 s | ~90 s |
B : Water = 3,0 % by weight Material Temperature | Increase in viscosity | Reaction time | +10 °C | ~56 s | ~110 s | +20 °C | ~37 s | ~68 s |
B : Water = 5,0 % by weight (standard mixture) Material Temperature | Increase in viscosity | Reaction time | +10 °C | ~50 s | ~80 s | +20 °C | ~28 s | ~40 s |
The data above are laboratory parameters and may deviate depending on the situation and conditions on site. |
The above design is only a sample of the options available, for reference purposes only. Our policy of continuous improvement may result in a change of specifications without notice. If any discrepencies might be between the data sheet values and standards, we reserve the rights to make technical changes. Our company will not be held responsible, as all or any of pictures, drawings, weights and dimensions details or other elements in this document are only indicative and must not be considered contractual. Contact our sales team for other specifications or custom made products.
Contact our sales team for other specifications or custom made products.